LEADER |
01486nam a2200253 a 4500 |
003 |
AR-SmUSM |
005 |
20191226125431.0 |
008 |
170315s1995 ne a b 000 0 eng d |
952 |
|
|
|0 0
|1 0
|2 ddc
|4 0
|6 676_270000000000000_H387_1995
|7 0
|8 GRAL
|9 62373
|a IIPC
|b IIPC
|d 2017-03-15
|e Donación
|l 1
|o 676.27 H387 1995
|p A01175
|r 2023-02-01 00:00:00
|s 2023-02-01
|w 2017-03-15
|y LIBRO
|
999 |
|
|
|c 43478
|d 43478
|
020 |
|
|
|a 9056130102
|
040 |
|
|
|a IIPC
|b spa
|c IIPC
|
082 |
0 |
|
|a 676.27
|b H387 1995
|2 20
|
100 |
1 |
|
|a Havermans, John.
|9 51782
|
245 |
1 |
0 |
|a Environmental influences on the deterioration of paper /
|c J. B. G. A. Havermans.
|
260 |
|
|
|a Rotterdam, Holanda :
|b Barjesteh, Meeuwes,
|c 1995.
|
300 |
|
|
|a x, 213 p. :
|b il. ;
|c 24 cm.
|
504 |
|
|
|a Incluye referencias bibliográficas.
|
505 |
2 |
|
|a Cap. 1.Introduction: Wood polymers ; Pulping, bleaching and papermaking ; Paper degradation ; Previous research projects on the effects of air pollutants -- cap. 2.Infrared spectroscopy as a tool for the characterization of paper and paper deterioration -- cap. 3.Studies on a naturally aged book -- cap. 4.A study of the ageing of paper in normal and inert environments -- cap. 5.Influences of SO2 and NOx on the accelerated ageing of paper -- cap. 6.Mass deacidification of archival materials DEZ.
|
650 |
|
7 |
|a Papel.
|2 unesco
|9 19281
|
650 |
|
7 |
|a Ingeniería ambiental.
|2 unesco
|9 2404
|
650 |
|
7 |
|a Tecnología de materiales.
|2 unesco
|9 5264
|
650 |
|
7 |
|a Libro raro.
|2 unesco
|9 2072
|
942 |
|
|
|2 ddc
|c LIBRO
|